Título: | Gradientes de umidade e suas implicações nas tensões de secagem, quantidade e dimensões de rachaduras na madeira de Eucalyptus tereticornis aos 15 anos |
Título(s) alternativo(s): | Moisture gradients and their implications on drying and quantity, crack dimensions on the wood of 15-year-old Eucalyptus tereticornis |
Autor(es): | Maiara Talgatti Amanda Grassmann da Silveira Talita Baldin Laura Hoffmann de Oliveira Elio José Santini |
Resumen: | O gradiente de umidade, que corresponde à diferença de umidade entre o centro e a periferia da peça de madeira, desempenha papel importante no desenvolvimento de tensões que causam defeitos como rachaduras, encruamento e empenamentos. Cuidados para reduzir essa diferença no decorrer e no final do processo de secagem são procedimentos importantes para que a qualidade da madeira não seja comprometida. O presente trabalho teve como objetivo avaliar o efeito do gradiente de umidade no desenvolvimento de tensões resultantes da secagem da madeira de Eucalyptus tereticornis conduzida em estufa convencional. Para isso, tábuas de 40 x 10 x 70 mm foram submetidas à secagem nas temperaturas de 45, 60 e 75°C, desde verde até o teor de umidade de 12%. No final da secagem foi avaliado a qualidade do material, por meio do gradiente de umidade, tensões de secagem e defeitos. A temperatura de 75ºC proporcionou menor tempo de secagem, porém, maiores gradientes de umidade, maiores tensões e menor qualidade da madeira ao final da secagem. As temperaturas de 60º e 40ºC apresentaram grande diferença no tempo de secagem, porém gradientes de umidade muito semelhantes e qualidade do material final também. Pode-se então, sugerir que seja utilizada a temperatura de 60ºC para a secagem da madeira de Eucalyptus tereticornis com ganho de tempo e qualidade muito próxima da proporcionada por baixas temperaturas. |
Abstract: | The moisture gradient, which corresponds to the humidity difference between the center and the periphery of the piece of wood plays an important role in the development of stresses that cause defects such as cracking, hardening and warping. Care to reduce this difference during and at the end of the drying process are important procedures so that the quality of the wood is not compromised. The present work had as the objective of this study was to evaluate the effect of the moisture gradient on the development of stresses of drying Eucalyptus tereticornis wood conducted in a conventional greenhouse. For 40 x 10 x 70 mm boards were then dried at temperatures of 45ºC, 60ºC and 75ºC, from green to a moisture content of 12%. At the end of the drying, the quality was evaluated. through the moisture gradient, drying stresses and defects. The temperature 75ºC provided shorter drying time, but higher moisture gradients, higher tensions and lower wood quality at the end of drying. The temperatures of 60ºC and 40ºC showed great difference in drying time, but humidity gradients very similar and quality of the fnal material as well. One can then suggest that it be 60ºC for drying Eucalyptus tereticornis wood with gain in time and quality very close to that provided by low temperatures. |
Asunto: | Eucalipto Madeira - Qualidade Madeira - Defeitos Madeira serrada - Secagem Madeira - Efeito da umidade |
Idioma: | por |
País: | Brasil |
Editor: | Universidade Federal de Minas Gerais |
Sigla da Institución: | UFMG |
Departamento: | ICA - INSTITUTO DE CIÊNCIAS AGRÁRIAS |
Tipo de acceso: | Acesso Aberto |
Identificador DOI: | 10.24278/2178-5031.201931106 |
URI: | http://hdl.handle.net/1843/46023 |
Fecha del documento: | jun-2019 |
metadata.dc.url.externa: | https://smastr16.blob.core.windows.net/iflorestal/2019/10/rif31-1_65-74.pdf |
metadata.dc.relation.ispartof: | Revista do Instituto Florestal |
Aparece en las colecciones: | Artigo de Periódico |
archivos asociados a este elemento:
archivo | Descripción | Tamaño | Formato | |
---|---|---|---|---|
Gradientes de umidade e suas implicações nas tensões de secagem, quantidade e dimensões de rachaduras na madeira de Eucalyptus tereticornis aos 15 anos.pdf | 441.27 kB | Adobe PDF | Visualizar/Abrir |
Los elementos en el repositorio están protegidos por copyright, con todos los derechos reservados, salvo cuando es indicado lo contrario.