Please use this identifier to cite or link to this item: http://hdl.handle.net/1843/BUBD-AFCM3W
Full metadata record
DC FieldValueLanguage
dc.contributor.advisor1Vanessa de Freitas Cunha Linspt_BR
dc.contributor.advisor-co1Hong Liangpt_BR
dc.contributor.referee1Luís Frederico Pinheiro Dickpt_BR
dc.contributor.referee2MARÍLIA MENDONÇA DE lIMA VALLOURECpt_BR
dc.contributor.referee3Wagner Reis da Costa Campospt_BR
dc.contributor.referee4Rosa Maria Rabelo Junqueirapt_BR
dc.creatorRenata Braga Soarespt_BR
dc.date.accessioned2019-08-11T16:28:05Z-
dc.date.available2019-08-11T16:28:05Z-
dc.date.issued2016-08-26pt_BR
dc.identifier.urihttp://hdl.handle.net/1843/BUBD-AFCM3W-
dc.description.abstractSupermartensitic stainless steels have recently been introduced in the oil and gas industries to substitute more expensive duplex stainless steels for onshore and offshore tubing applications. This work aimed at evaluating the corrosion and tribocorrosion behavior of supermartensitic steels for application in oil and gas industry in aqueous media containing chlorides. The steel microstructure was characterized using optical microscopy (OM), scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), interferometry, X-ray diffraction (XRD), Mössbauer and electron backscattered diffraction (EBSD). The electrochemical characterization on steel surface supermatensitic stainless steel has been studied using potentiodynamic anodic polarization, cyclic potentiodynamic polarization, electrochemical impedance spectroscopy (EIS), Mott-Schottky and scanning vibrating electrode technique (SVET). A tribocorrosion setup was configured in order to study the triboelectrochemical behavior of a supermartensitic steel. Wear analysis indicated that three-body abrasion was the dominant wear mechanism. Due to the synergetic effect of wear and corrosion, the concentration of pits was higher with rubbing but the pit propagation was inhibited. The smallest abrasive particles promoted the highest pit growth inhibition. The effect of larger diamond particles on tribocorrosion of supermartensitic steel would be less harmful than the effect of smaller abrasive particles. Coarse cuboidal TiN particles were identified on the steel surfaces of all samples. The TiN inclusions showed microvoids and a nucleous containing magnesium, aluminum and calcium oxides. Mössbauer analysis identified 0.7, 0.5 and 0.9% of retained austenite in SMSS samples as-quenched and tempered at 600oC and 640oC, respectively. The sample tempered at 600oC showed the lowest grain size, evaluated by using EBSD technique, and the highest localized corrosion resistance in a saline medium. The SMSS sample tempered at 640oC showed no electrochemical activity after 3600s of immersion in a saline solution by using a SVET technique, but after 86400s, a pit was detected. SVET analysis showed the association of a localized corrosion sites with the TiN inclusion on the steel surface. The 0.6 mol/L NaCl aqueous solution was the less aggressive electrolyte to the supermartensitic stainless steel (SMSS). The SMSS tempered at 600°C exhibited the highest corrosion resistance in two electrolytes. Furthermore, the capacitance study shows that the passive films formed on supermartensitic steel behave as p-type semiconductors below the flat band potential.pt_BR
dc.description.resumo...pt_BR
dc.languagePortuguêspt_BR
dc.publisherUniversidade Federal de Minas Geraispt_BR
dc.publisher.initialsUFMGpt_BR
dc.rightsAcesso Abertopt_BR
dc.subjectEngenharia Químicapt_BR
dc.subject.otherAço Indústriapt_BR
dc.subject.otherEngenharia quimicapt_BR
dc.subject.otherAço inoxidável Corrosãopt_BR
dc.titleResistência à corrosão e à tribocorrosão de aços inoxidáveis supermartensíticos utilizados na indústria de petróleo e gáspt_BR
dc.typeTese de Doutoradopt_BR
Appears in Collections:Teses de Doutorado

Files in This Item:
File Description SizeFormat 
thesis_renata_2016.pdf8.67 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.