The effect of initial strain in the severe plastic deformation of aluminum on the subsequent work hardening regeneration through low strain amplitude multi-directional forging

dc.creatorCleber Granato de Faria
dc.creatorNatanael Geraldo e Silva Almeida
dc.creatorKarla Balzuweit
dc.creatorMaria Teresa Paulino Aguilar
dc.creatorPaulo Roberto Cetlin
dc.date.accessioned2025-02-26T15:27:57Z
dc.date.accessioned2025-09-09T00:25:40Z
dc.date.available2025-02-26T15:27:57Z
dc.date.issued2021
dc.description.sponsorshipCNPq - Conselho Nacional de Desenvolvimento Científico e Tecnológico
dc.description.sponsorshipCAPES - Coordenação de Aperfeiçoamento de Pessoal de Nível Superior
dc.identifier.doihttps://doi.org/10.1016/j.matlet.2021.129462
dc.identifier.issn1873-4979
dc.identifier.urihttps://hdl.handle.net/1843/80459
dc.languageeng
dc.publisherUniversidade Federal de Minas Gerais
dc.relation.ispartofMaterials Letters
dc.rightsAcesso Restrito
dc.subjectAlumínio
dc.subjectMicroestrutura
dc.subject.otherAluminum
dc.subject.otherSevere plastic deformation
dc.subject.otherMulti-directional forging
dc.subject.otherMicrostructures
dc.subject.otherWork hardening
dc.titleThe effect of initial strain in the severe plastic deformation of aluminum on the subsequent work hardening regeneration through low strain amplitude multi-directional forging
dc.typeArtigo de periódico
local.citation.epage5
local.citation.spage1
local.citation.volume290
local.description.resumoWork hardening caused by Severe Plastic Deformation (SPD) strengthens ductile metals remarkably but practically annihilates their further work hardening during monotonic post-SPD deformation. Low Strain Amplitude Multi-Directional Forging (LSA-MDF) after one Equal Channel Angular Pressing (ECAP) pass of aluminum causes limited softening and regenerates its work hardening capacity. The full development of an SPD condition in aluminum demands an initial deformation higher than that associated with one ECAP pass. The present research analyzes the application of LSA-MDF to aluminum after 4 ECAP passes. A regeneration of the work hardening capacity of the material was observed. In addition, LSA-MDF caused an increased fraction of High Angle Grain Boundaries (HAGBs) in the material and a decrease in the presence of distorted grains displaying internal dislocation structures.
local.identifier.orcidhttps://orcid.org/0000-0003-0845-9847
local.identifier.orcidhttps://orcid.org/0000-0001-7124-4545
local.identifier.orcidhttps://orcid.org/0000-0002-0121-0881
local.identifier.orcidhttps://orcid.org/0000-0002-8051-062X
local.publisher.countryBrasil
local.publisher.departmentENG - DEPARTAMENTO DE ENGENHARIA MATERIAIS E DA CONSTRUÇÃO CIVIL
local.publisher.departmentENG - DEPARTAMENTO DE ENGENHARIA MECÂNICA
local.publisher.departmentICX - DEPARTAMENTO DE FÍSICA
local.publisher.initialsUFMG
local.url.externahttps://www.sciencedirect.com/science/article/pii/S0167577X21001580?via%3Dihub