Effect of indirect restorative material and thickness on light transmission at different wavelengths
Carregando...
Data
Título da Revista
ISSN da Revista
Título de Volume
Editor
Universidade Federal de Minas Gerais
Descrição
Tipo
Artigo de periódico
Título alternativo
Primeiro orientador
Membros da banca
Resumo
Purpose: The aim of this study was to evaluate the influence of indirect restorative material type and thickness on the transmission of different wavelengths from a broad-banded dental curing light.
Methods: Four dental indirect restorative materials for computer-aided design and computer-aided manufacturing (CAD/CAM) were evaluated: [RC] resin/ceramic hybrid material (Lava Ultimate), [FC] feldspathic ceramic (VitaBlocs), and two zirconia-based ceramics ([ZK] Katana; and [ZL] Lava). Total loss of irradiance (TL) was measured for blue (WB, 425-490nm) and violet (WV, 350-425nm) wavelengths. Specimens of 15×15mm with varying thicknesses (0.5, 1.0, 1.5, and 2.0mm) were fabricated (n=5). A plasma-arc dental light-curing unit was used (Arc Light-II). To assess TL as a function of wavelength, a software (Spectra Suite v5.1) connected to a spectroradiometer (USB2000) and an integrating sphere (CTSM-LSM-60-SF) was used. Data was subjected to statistical analysis (two-way ANOVA and post-hoc Tukey test, α=0.05).
Results: A 0.5mm interposition resulted in TL from 50.5 to 67.2%, depending on material. Increased thickness resulted in higher TL for all materials. FC showed less TL compared to ZK. In general, WV showed higher TL than did WB, and WV/WB proportion decreased with increasing thickness.
Conclusions: Indirect materials significantly reduced TL, and this effect is greater with increasing thickness. WV showed lower penetration compared to WB
Abstract
Assunto
Ceramics, Composite resins
Palavras-chave
Ceramics, Composite, Irradiance, Photopolymerization, Zirconia