Análise de argamassas de revestimento produzidas com rejeito de minério de ferro

dc.creatorSofia Araujo Lima Bessa
dc.creatorIsabela Karoline Mendonça
dc.creatorJhade Vimieiro
dc.creatorGleisson Gurgel
dc.creatorLuciano Magalhães
dc.creatorAugusto Cesar da Silva Bezerra
dc.creatorRejane Magiag Loura
dc.date.accessioned2024-01-09T18:08:27Z
dc.date.accessioned2025-09-09T00:48:32Z
dc.date.available2024-01-09T18:08:27Z
dc.date.issued2018
dc.format.mimetypepdf
dc.identifier.issn2178-8960
dc.identifier.urihttps://hdl.handle.net/1843/62518
dc.languagepor
dc.publisherUniversidade Federal de Minas Gerais
dc.relation.ispartofEncontro Nacional de Tecnologia do Ambiente Construído
dc.rightsAcesso Aberto
dc.subjectConstrução civil
dc.subjectArgamassa
dc.subjectMinérios de ferro
dc.subjectPropriedades mecanicas
dc.subject.otherCoating mortars
dc.subject.otherIron ore tailings
dc.subject.otherMechanical properties
dc.titleAnálise de argamassas de revestimento produzidas com rejeito de minério de ferro
dc.typeArtigo de evento
local.citation.epage2772
local.citation.issue17 ENTAC - Encontro Nacional de Tecnologia do Ambiente Construído
local.citation.spage2765
local.description.resumoMining is one of the main sectors for the Brazilian economy and the state of Minas Gerais accounts for 35% of Brazilian mining. However, ore mining generates thousands of tons per day of diferents liquid, solid and sludge wastes. In this work, the objective was to replace part of Portland cement (PC) for calcined and raw iron ore tailings (IOT) in the production of cementlime mortars. Mortars were produced with PC, hydrated lime and sand, using a constant 1:2:9 (weight basis). The IOT samples were used in a raw state and also calcined at 500°C, both ground for 10 minutes. The cement was replaced by IOT in the following percentages: 0%, 10%, 20%, 40% and 60%. The water/binder ratio of each mortar was determined by the consistency index. Cylindrical specimens were molded to determine the water absorption by immersion, borehole index and bulk density, at 28 days. For the flexural tensile strength test, 40x40x160mm prismatic specimens were molded. All specimens remained in the mold for 48 hours and, after demolding, they were cured in a laboratory environment until the test date. The results showed that the substitution of the PC for IOT, until 60% in mortars, didn't modify their properties.
local.identifier.orcidhttps://orcid.org/0000-0002-7048-8035
local.publisher.countryBrasil
local.publisher.departmentARQ - DEPARTAMENTO DE TEC ARQUITETURA E URBANISMO
local.publisher.initialsUFMG
local.url.externahttps://drive.google.com/file/d/1EOfjTvkXL7aqgK9y5wqPamRSLsa3D-1V/view

Arquivos

Pacote original

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
Análise de argamassas de revestimento produzidas com rejeito de minério de ferro.pdf
Tamanho:
3.36 MB
Formato:
Adobe Portable Document Format

Licença do pacote

Agora exibindo 1 - 1 de 1
Carregando...
Imagem de Miniatura
Nome:
License.txt
Tamanho:
1.99 KB
Formato:
Plain Text
Descrição: