Thermal, vibrational and optical properties of PrLuO3 interlanthanides from hydrothermally-derived precursors
Carregando...
Data
Título da Revista
ISSN da Revista
Título de Volume
Editor
Universidade Federal de Minas Gerais
Descrição
Tipo
Artigo de periódico
Título alternativo
Primeiro orientador
Membros da banca
Resumo
PrLuO3 interlanthanides were prepared at temperatures ranging from 800 °C to 1600 °C using hydrothermally-derived precursors. The chemical reactions observed include the conversion and segregation of Pr(OH)3 and LuO(OH), respectively, into PrO2 and Lu2O3 cubic oxides below 1200 °C, followed by the production of a mixture of hexagonal P63/mmc and orthorhombic Pnma PrLuO3 phases at 1400 °C. Phase-pure orthorhombic PrLuO3 was obtained at 1600 °C, which was corroborated by Raman and micro far-infrared spectroscopic analyses. Photoluminescence, colorimetric and lifetime measurements were carried out in PrLuO3 samples. Dominant emission verified in samples calcined at 1400 °C corresponds to the hypersensitive 3P0 → 3F2 transition with a color purity of 97% (decay times of 12 μs and 3 μs), while emissions for the phase-pure samples correspond to the 3P0 → 3H6 and 3P0 → 3H5 transitions with a color purity of 94% (a single luminescence lifetime of 12 μs). The optical properties of PrLuO3 interlanthanides thereby suggest that they can be used as luminescent materials in both structural arrangements.
Abstract
Assunto
Metais de terras raras, Espectroscopia de infravermelho, Raman, Espectroscopia de, Fotoluminescência
Palavras-chave
Interlanthanides, Hydrothermally-derived precursors, Conversion, Segregation, Raman spectroscopic, Infrared spectroscopic