Title: Evolução do tamanho de grão e comportamento mecânico do magnésio comercialmente puro submetido a tratamento termo-mecânico de ECAP
Authors: Claudio Laudares Passos Silva
First Advisor: Roberto Braga Figueiredo
First Referee: Maria Teresa Paulino Aguilar
Second Referee: Paulo Roberto Cetlin
Abstract: No presente trabalho amostras de magnésio comercialmente puro foram processadas por deformação plástica severa por ECAP (Equal Channel Angular Pressing), em temperaturas moderadas, utilizando uma matriz com ângulo de interseção entre canais = 135°. Para realizar o processamento, sem danificar o material, as amostras passaram por uma etapa intermediária de processamento por laminação e foram cobertas com uma fina camada de cobre para reduzir o atrito com as paredes internas da matriz. Foram realizados quatro passes pela matriz seguindo a rota de processamento C com uma taxa de prensagem de 10 mm/min. Por meio de metalografia foi feita a análise da microestrutura do material em cada etapa de processamento. Assim foi verificado que o material laminado com redução de 5 mm para 1 mm de espessura, após o quarto passe de ECAP, apresentava um estrutura de grãos homogênea e completamente refinada com tamanho médio de grão igual a 5 m. Foram feitos ensaios de tração para determinar o comportamento mecânico do material antes e após o processamento por ECAP, nesses ensaios foi possível verificar um aumento da ductilidade após o processamento por ECAP. O coeficiente de sensibilidade à taxa de deformação m foi determinado a partir das curvas de tensão verdadeira versus deformação verdadeira obtidas nos ensaios de tração do material laminado e do material processado por laminação e ECAP. Os valores de m determinados para o material laminado e para o material processado por ECAP apresentaram valores muito próximos.
Abstract: In this work samples of commercially pure magnesium were processed by ECAP (Equal Channel Angular Pressing), in moderate temperatures, using a die with angle of = 135° between the two channels. An intermediate step of rolling was used to facilitate the processing and to avoid cracking, the samples was covered with a cooper sheet of 0.3 mm thickness to reduce friction between the sample and the die channel. The samples were processed by 4 steps of ECAP using route C, with punch speed of 10 mm/min. The microstructure of the material was evaluated using metallographic procedures. The material processed by rolling from 5 mm to a thickness of 1 mm + ECAP (4 steps) exhibits a completely refined and homogeneous microstructure with average grain size of 5 m. Tensile tests were used to determine mechanical behavior after and before ECAP and show an increase in ductility of the material processed by ECAP. The strain rate sensitivity coefficient was determined by true stress versus true strain curves obtained in the tensile tests of the material processed by rolling and the material processed by rolling and ECAP. The m values determined for the rolled material and for the material processed by ECAP were very similar.
Subject: Materiais de construção
Magnesio
Construção civil
language: Português
Publisher: Universidade Federal de Minas Gerais
Publisher Initials: UFMG
Rights: Acesso Aberto
URI: http://hdl.handle.net/1843/BUBD-A2SJL5
Issue Date: 16-Jan-2015
Appears in Collections:Dissertações de Mestrado

Files in This Item:
File Description SizeFormat 
dissertacao_de_mestrado__cl_udio_laudares___21_04_15_.pdf28.21 MBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.